Longevity of Bonding of Self-adhesive Resin Cement to Dentin

dc.contributor.authorSimoes, T. C.
dc.contributor.authorLuque Martínez, Íssis Virginia
dc.contributor.authorMoraes, R. R.
dc.contributor.authorSa, A. T. G.
dc.contributor.authorLoguercio, A.
dc.contributor.authorMoura, S. K.
dc.date.accessioned2019-10-16T20:16:10Z
dc.date.available2019-10-16T20:16:10Z
dc.date.issued2016
dc.description.abstractObjective: To evaluate the effect of root dentin treatment on the bonding of self-adhesive resin cement after 24 hours and after 6 months. Methods: A total of 48 single-rooted premolars were endodontically treated and divided into four groups (n=12): Adper Scotchbond Multi-Purpose + RelyX ARC (ARC); RelyX U200 (U200); EDTA + RelyX U200 (EU200); and phos-phoric acid (H3PO4) + RelyX U200 (HU200). After filling the roots, an Exacto No. 2 fiber post was cleaned, treated with silane (60 seconds), positioned, and light cured (LED; 60 seconds at 1200 mW/cm(2)). After storage (37 degrees C/24 h), the roots were cut to obtain two discs (1 mm) of each third. They were stored in distilled water (24 hours at 37 degrees C); one disc of each root-third was subjected to the push-out test (0.5 mm/min) at 24 hours and the other disc after six months of water storage (37 degrees C). The data on the root-thirds were averaged for statistical purposes. The average values of bond strength (MPa) were analyzed by twoway analysis of variance and post hoc Student-Newman-Keuls (5%). Results: There were statistical differences for the treatment of dentin (p<0.001), for time (p=0.003), and the interaction of treatment and time (p=0.017). After 24 hours, we observed lower bond strength in the HU200 group when compared with other groups (ARC, U200, and EU200). After six months, HU200 showed the lowest bond strength. Higher strengths were observed for EU200 and U200 similarly, which were higher than ARC. Conclusion: The bonding of the self-adhesive resin cement varied over time in the tested groups.
dc.format.extent9 páginas
dc.fuente.origenFacultad de Medicina
dc.identifier.doi10.2341/14-266-LR
dc.identifier.issn0361-7734
dc.identifier.urihttps://repositorio.uc.cl/handle/11534/26567
dc.identifier.urihttps://doi.org/10.2341/14-266-LR
dc.issue.numeroNo. 3
dc.pagina.finalE72
dc.pagina.inicioE64
dc.revistaOperative Dentistryes_ES
dc.rightsacceso abierto
dc.subjectdemineralized human dentines_ES
dc.subjectglass-fiber postses_ES
dc.subjectsmear layeres_ES
dc.subjectroot Canalses_ES
dc.subjectretentiones_ES
dc.subjectstrengthes_ES
dc.subjectenameles_ES
dc.subjectresistancees_ES
dc.subjectcollagenes_ES
dc.subjectsystemses_ES
dc.subjectDentistry, Oral Surgery & Medicinees_ES
dc.subject.ddc610
dc.subject.deweyMedicina y saludes_ES
dc.titleLongevity of Bonding of Self-adhesive Resin Cement to Dentines_ES
dc.typeartículo
dc.volumenVol. 41
sipa.codpersvinculados1020227
Files
Original bundle
Now showing 1 - 1 of 1
Loading...
Thumbnail Image
Name:
Longevity of Bonding of Self-adhesive Resin Cement to Dentin.pdf
Size:
706.49 KB
Format:
Adobe Portable Document Format
Description: